Properties of Metallic Yarn
Metallic yarn have the following chemical characteristics
Ironing 15 sec at 110°C
Dry Heat 60 sec at 180°C
Alkali, solution of 1st process 30 min at pH 4.7
Hot water 30min at 90°C
Hand washing 0.5% soap, 0.2% sodium carbondate anhydride, 30 min at 60°C
Rubbing 200g, 100 time
Dry cleaning trichloroethylene, perchloroethylene or petroleum benzene; 30min at 25°C
Steaming 40min at 100°C
Boiling water 30-60 min
Acid 2% oxalic adic or 2% acetic acid for 10min at 60°C
Scouring for supports / twists of metallic yarn Soda Ash, 1 g/l for 30min at 60°C
Customs tariff number 5605.00.100